yxpolyer PPS-TF Natural 1.75mm 1kg

yxpolyer PPS-TF Natural 1.75mm 1kg

8,030 kr
Skip to product information
yxpolyer PPS-TF Natural 1.75mm 1kg

yxpolyer PPS-TF Natural 1.75mm 1kg

8,030 kr

PPS-TF (Tensile-Enhanced Polyphenylene Sulfide) is an impact-modified variant of PPS engineered for improved toughness while retaining the hallmark advantages of the base polymer. Like standard PPS it offers a continuous service temperature of 220-240°C and resists virtually all solvents below 200°C. The tensile enhancement raises impact resistance above that of unfilled PPS making it more robust for structural parts subject to occasional shock loads. It remains extremely hard (harder than PC and most nylons) and very stiff. Requires a high-temperature hotend capable of 290-330°C, a heated bed at 100-110°C, and an enclosure with an ambient chamber temperature around 70°C. Parts should be tempered at ≥130°C immediately after printing to lock in maximum strength; higher annealing temperatures (up to 200°C) yield progressively stronger parts. Despite PPS absorbing very little moisture, hot drying is recommended before printing because what little moisture it does absorb is difficult to drive out at lower temperatures.

📊 Technical Specifications

Nozzle Temperature 290-330 °C
Bed Temperature 100-110 °C
Print Speed 25-100 mm/s *
Part Cooling Fan 0-10 % *
Max Volumetric Speed 25 mm³/s *
Drying Temperature 100 °C *
Drying Time 6 hours *
Enclosure Required Yes
Tensile Strength (Yield, XY) 57 MPa
Tensile Strength (Yield, Z) 31.4 MPa *
Tensile Strength (Break, XY) 57 MPa
Tensile Strength (Break, Z) 31.4 MPa *
Tensile Modulus (XY) 3800 MPa *
Tensile Modulus (Z) 2280 MPa *
Elongation at Break 2.5 %
Flexural Strength (XY) 95 MPa
Flexural Strength (Z) 27 MPa
Flexural Modulus (XY) 3185 MPa
Flexural Modulus (Z) 2210 MPa
Impact Strength (Izod) 30 J/m *
Impact Strength (Unnotched, XY) 25 kJ/m²
Impact Strength (Unnotched, Z) 3 kJ/m²
Heat Deflection (0.45 MPa) 110 °C
Heat Deflection (1.8 MPa) 110 °C *
Glass Transition (Tg) 90 °C *
Melting Point 300 °C
Density 1.4 g/cm³
Hardness (Shore A) 50.4 *
Hardness (Shore D) 56.4 *
Hardness (Rockwell R) 124 *
Continuous Service Temp 220 °C *
Light Transmittance 0 % *
Dielectric Strength 18 kV/mm *
Impact Strength (Charpy) 4 kJ/m² *
Elongation at Yield 3 % *
Mold Shrinkage 0-0 % *
Water Absorption (24h) 0.1 %
Flammability Rating V-0
Bed Adhesion Nano Polymer *

* Estimated values based on material family characteristics