Yasin POM Natural 1.75mm 1kg

Yasin POM Natural 1.75mm 1kg

4.310 kr
Skip to product information
Yasin POM Natural 1.75mm 1kg

Yasin POM Natural 1.75mm 1kg

4.310 kr

POM (Polyacetal/Delrin) is an engineering thermoplastic famous for its extremely low coefficient of friction and excellent dimensional stability. Widely used in gears bearings and sliding mechanisms where low wear and smooth motion are critical. Warning: produces formaldehyde fumes during printing - requires excellent ventilation.

📊 Technical Specifications

Nozzle Temperature 210-230 °C *
Bed Temperature 110-130 °C *
Print Speed 30-50 mm/s *
Part Cooling Fan 0 % *
Max Volumetric Speed 12 mm³/s *
Drying Temperature 70-80°C *
Drying Time 4 hours *
Enclosure Required Yes *
Tensile Strength (Yield, XY) 65 MPa *
Tensile Strength (Yield, Z) 29.2 MPa *
Tensile Strength (Break, XY) 45 MPa *
Tensile Strength (Break, Z) 20.2 MPa *
Tensile Modulus (XY) 2800 MPa *
Tensile Modulus (Z) 1680 MPa *
Elongation at Break 35 % *
Flexural Strength (XY) 85 MPa *
Flexural Strength (Z) 46.8 MPa *
Flexural Modulus (XY) 2600 MPa *
Flexural Modulus (Z) 1690 MPa *
Impact Strength (Izod) 60.0 J/m *
Impact Strength (Unnotched, XY) 24 kJ/m² *
Impact Strength (Unnotched, Z) 9.6 kJ/m² *
Heat Deflection (0.45 MPa) 110 °C *
Heat Deflection (1.8 MPa) 110 °C *
Glass Transition (Tg) -30 °C *
Melting Point 165-175 °C *
Density 1.4 g/cm³ *
Hardness (Shore A) 52 *
Hardness (Shore D) 54.5 *
Hardness (Rockwell R) 120 *
Continuous Service Temp 100 °C *
Light Transmittance 0 % *
Dielectric Strength 20 kV/mm *
Impact Strength (Charpy) 6 kJ/m² *
Elongation at Yield 10 % *
Mold Shrinkage 2-2 % *
Water Absorption (24h) 0.2 % *
Flammability Rating HB *
Bed Adhesion Wood Glue *

* Estimated values based on material family characteristics