yxpolyer ASA (Acrylonitrile Styrene Acrylate) offers similar properties to ABS but with exceptional UV resistance making it the premier choice for outdoor applications. Weather-resistant parts maintain color and mechanical properties under prolonged sun exposure where ABS would degrade. Prints similarly to ABS but with slightly reduced warping tendency.

📊 Technical Specifications

Nozzle Temperature 240-260 °C *
Bed Temperature 90-110 °C *
Print Speed 40-60 mm/s *
Part Cooling Fan 0-10 % *
Max Volumetric Speed 14.4 mm³/s *
Drying Temperature 80 °C *
Drying Time 4 hours *
Enclosure Required Yes *
Tensile Strength (Yield, XY) 46 MPa *
Tensile Strength (Yield, Z) 34.5 MPa *
Tensile Strength (Break, XY) 46 MPa *
Tensile Strength (Break, Z) 34.5 MPa *
Tensile Modulus (XY) 2350 MPa *
Tensile Modulus (Z) 1880 MPa *
Elongation at Break 30 % *
Flexural Strength (XY) 75 MPa *
Flexural Strength (Z) 63.8 MPa *
Flexural Modulus (XY) 2350 MPa *
Flexural Modulus (Z) 1927 MPa *
Impact Strength (Izod) 147 J/m *
Impact Strength (Unnotched, XY) 60 kJ/m² *
Impact Strength (Unnotched, Z) 42 kJ/m² *
Heat Deflection (0.45 MPa) 98 °C *
Heat Deflection (1.8 MPa) 87 °C *
Glass Transition (Tg) 100 °C *
Melting Point 90-130 °C *
Density 1.1 g/cm³ *
Hardness (Shore A) 58.8 *
Hardness (Shore D) 46.8 *
Hardness (Rockwell R) 103 *
Continuous Service Temp 84 °C *
Light Transmittance 80 % *
Dielectric Strength 22 kV/mm *
Impact Strength (Charpy) 15 kJ/m² *
Elongation at Yield 5 % *
Mold Shrinkage 0-0 % *
Water Absorption (24h) 0.3 % *
Flammability Rating HB *
Bed Adhesion ABS Adhesive *

* Estimated values based on material family characteristics